Go ![]() | New ![]() | Find ![]() | Notify ![]() | Tools ![]() | Reply ![]() | ![]() |
One of Us |
I cant find the small tubes of two part devcon plastic steel localy anymore, no one carries it anymore Found midway has it in one pounders Question is: Is this 2 jars(2 part) One jar of resin and one jar of hardener? Or is this different than the 2 part stuff? ![]() | ||
|
one of us![]() |
I "believe" that picture is the jar of part "A" there should also be a "B" As usual just my $.02 Paul K | |||
|
Moderator |
please give marinetex grey a shot opinions vary band of bubbas and STC hunting Club Words aren't Murder - Political assassination is MURDER Information on Ammoguide about the416AR, 458AR, 470AR, 500AR What is an AR round? Case Drawings 416-458-470AR and 500AR. 476AR, http://www.weaponsmith.com | |||
|
One of Us![]() |
Jeffy, who handles Marinetex grey? ![]() Olcrip, Nuclear Grade UBC Ret. NRA Life Member, December 2009 Politicians should wear Nascar Driver's jump suites so we can tell who their corporate sponsers are! | |||
|
One of Us |
Thanks Paul This is the stuff ive used before, and it is "good shit" . It has a #62345, and is black when mixed and hard ![]() Is it the same stuff im going to use it this time on back side of some Old black Plastic Single action revolver grips off a Herters powermag to repair the locator pin boss and stop anymore cracking | |||
|
One of Us |
Jeff, I had some marine tex years ago, put cant find a local supplier either. Gotta mail order every damn thing anymore ![]() | |||
|
Moderator |
Brown ells and most boat and marineshops. The white is softer, alot opinions vary band of bubbas and STC hunting Club Words aren't Murder - Political assassination is MURDER Information on Ammoguide about the416AR, 458AR, 470AR, 500AR What is an AR round? Case Drawings 416-458-470AR and 500AR. 476AR, http://www.weaponsmith.com | |||
|
One of Us![]() |
I'm just about out of Accra-gel. I will order a batch of Marinetex from Montizuma to see how it performs for me. Can a guy use atomized Stainless Steel with it? ![]() Olcrip, Nuclear Grade UBC Ret. NRA Life Member, December 2009 Politicians should wear Nascar Driver's jump suites so we can tell who their corporate sponsers are! | |||
|
one of us |
If you can't find Devcon, just use JB Weld from the auto parts stores. It's a steel filled epoxy too. | |||
|
Moderator |
I guess you could. I do big bores, up to 550s with it. opinions vary band of bubbas and STC hunting Club Words aren't Murder - Political assassination is MURDER Information on Ammoguide about the416AR, 458AR, 470AR, 500AR What is an AR round? Case Drawings 416-458-470AR and 500AR. 476AR, http://www.weaponsmith.com | |||
|
One of Us |
Here in Aus i buy the Devcon in pots like your picture. It will come in a box, the big pot like your picture will be the filler, there will be a small pot with hardener, they are NOT mixed at 50/50 like the other tube stuff. I use the liquid, Stock #10210. Paz 458AR & 500AR owner (yes it is done ![]() 12GFH in the pipeline(but not a real one, just a "mini one"!! The single shot on fine and beautiful lines built by a master craftsman is indeed a gentleman's piece... Colonel Townsend Whelen | |||
|
One of Us![]() |
I have used J-B weld and it works, but I like the Devcon 10110 better. I find it easier to work with, it's more paste and less runny. I use a scale to get the mix right. I am able to get it at my local industrial supply store. It doesn't age fast (it will last for 1 or 2 years) and there is enough to do 8 to 10 guns........Tom SCI lifer NRA Patron DRSS DSC | |||
|
One of Us |
I prefer marine tex bed today shoot tomorrow | |||
|
one of us |
When you are REALLY sure you are set up for the bedding, try Devcon Titanium. I got some on recommendation from Iron Brigade Armory years ago. Unbelievable stuff, and not just the price... ![]() | |||
|