posted Hide Post
no problem just use a bit of block heat
 
Posts: 13462 | Location: faribault mn | Registered: 16 November 2004Reply With Quote
One of Us
Picture of dpcd
posted Hide Post
You wont be applying that much heat to it; just tig it up. It was too hard to start with so a bit of tempering in that area will/might help.
 