I see alot of scope rings and bases are made of 12L14,and left unhardened(I'm assuming since they don't look case hardened). But I know some custom rings are hardened steel. So what should I use for making a set of rings and bases of my own? Just use cold rolled or should I get some 1045 or 4140? Same question applies to bottom metal Just use cold rolled low carbon or should I use something I can harden? Any opinions much appreciated.
 
Posts: 93 | Registered: 14 October 2003Reply With Quote
Moderator
Picture of jeffeosso
posted Hide Post
wanna,
1018/1020 is fine for this...
jeffe
 
Posts: 40016 | Location: Conroe, TX | Registered: 01 June 2002Reply With Quote
one of us
posted Hide Post
I'd go with 12L14 or 303 s.s. I really hate 1018 or 1020 CRS, too much residual stresses in the material.
Just my opinion......
 
Posts: 275 | Location: NW USA | Registered: 27 May 2001Reply With Quote
Moderator
Picture of jeffeosso
posted Hide Post
Jay,
i can agree with that... so go with hotroll?

iirc, 12L14 is leaded... which I don't really want to machine in my shop... even though it turns VERY nicely

jeffe
 
Posts: 40016 | Location: Conroe, TX | Registered: 01 June 2002Reply With Quote