The Accurate Reloading Forums
Heat treating an action

This topic can be found at:
https://forums.accuratereloading.com/eve/forums/a/tpc/f/9411043/m/745109021

29 February 2004, 17:59
Lar45
Heat treating an action
Hi all, I picked up an old Hopkins and Allen falling block 12ga shotgun action. The thought here is to make a heavy slug gun out of it. I rockwell tested the action and it is 65 on the B scale. Seems pretty soft. I've calculated yield and shear based on hot rolled 1020 and came up with a max chamber pressure of 17ksi with 100% saftey factor. I couldn't find a reference on how to calculate shear in threads though. 1.1" OD x 1.8" shank. I'm guessing half the peak of the thread so OD x PI x 1.8/2?? for shear area? Anyway, I'd like to heat treat the action to increase the strength, but I don't know exactly what kind of steel it's made out of that's why I went with 1020. Is there anyway to findout what it's made of?

Thoughts?
01 March 2004, 03:58
<Guest>
Most larger heat treating facilities have metallurgical services available. they will shave off a tiny piece of steel from your action and chemically analyze it for you.

Blue
01 March 2004, 05:24
Nitroman
Lar,

Send me a small piece of the steel and I'll shoot it in the electron microscope and return a printout of the chemical makeup of the steel.
01 March 2004, 05:34
Lar45
Nitroman, email sent
05 March 2004, 00:31
irv
lar45, What force in the action would act to shear the threads, other than the "drag" of the bullet?,
Take Care!