The Accurate Reloading Forums
niter bluing question

This topic can be found at:
https://forums.accuratereloading.com/eve/forums/a/tpc/f/9411043/m/192100018

06 February 2008, 22:58
tin can
niter bluing question
I see in Kuhnhausen's "The Mauser Bolt Actions" a table of temperatures using niter bluing that produce different colors- my question is would this range of temperatures, 430º-640ºF, louse up the heat treating on a Mauser extractor?

also, am I correct in thinking the extractor is "spring tempered"?
07 February 2008, 00:30
gunmaker
Spring temper is a little higher than that. The Brits used to use a lead pot to temper springs with. Lead melts near the top end of your tempering colors.


gunmaker
------------------
James Anderson Metalsmith & Stockmaker
WEB SITE

More Pics on FLICKR
07 February 2008, 00:41
tin can
thanks- so, it appears to be safe to use the niter process on an extractor. actually, the colors I would be after are in the mid-range, not towards the top.

the Brits used the lead pot method on cavalry swords, also, around the last 25 years of the 19th century and into the twentieth- kind of a "product needed to match the technology" deal, tempering swords which were undoubtedly on their way out of use.
07 February 2008, 04:42
Duane Wiebe
You can buy all he stuff you need from Brownells and in the bargain learn everything you didn't want to know about nitre bluing..bear in mind it's about the most fragile of the bluing process' Not much more than heat bluing made complicated