01 October 2005, 11:34
stuntpilot2African Grand Slam Tungsten cored Solids in 460 WBY
Has anyone loaded the tungsten carbide cored solid versions up to maximum in their 460 WBY? If you wouldn't mind sharing the details with me, especially where you began to encounter bolt stickiness or primer extrusion, I'd appreciate it. Thanks in advance.
Best Regards,
Stuntpilot
02 October 2005, 03:39
AtkinsonI was told by a very well known and old PH that he used them in his .460 Wby and had several of them break in half...so he went to using monolithic solids...I trust his judgement...
02 October 2005, 06:47
WillI've used the Solids in the Lott and 458 WM with good success, but they were at less than 460 velocities.
09 October 2005, 11:36
stuntpilot2quote:
Originally posted by Atkinson:
I was told by a very well known and old PH that he used them in his .460 Wby and had several of them break in half...so he went to using monolithic solids...I trust his judgement...
That's sobering. Especially given their price. Thanks for the data!
Stuntpilot