The Accurate Reloading Forums
Chamber Reaming 375 H&H

This topic can be found at:
https://forums.accuratereloading.com/eve/forums/a/tpc/f/4711043/m/45010517

25 April 2001, 17:39
rcasto
Chamber Reaming 375 H&H
I recently purchased a PPG reamer in 375 H&H in order to make Wilson-type chamber seating die. Fortunately I have the help of my uncle, a retired tool and die maker. However, he has never had to use a tapered reamer and has never cut a rifle chamber. My question is: How much metal can these reamers be expected to remove? It seems to me that if after drilling a .377 pilot hole, the reamer would suffer tremendous wear if a series of larger holes were not drilled first. Any help is appreciated.
26 April 2001, 02:17
<DuaneinND>
The reamer you have is quite capable of doing the entire job, the only drawback being it will take a fair amount of time do to having to remove and clear the chips every .050-.100 depending on how the reamer handles the chip load. Many rifle barrels are chambered completely with only a finish reamer.